Return
to DOE Report Table of Contents - S
An Attrition-Resistant Zinc
Titanate Sorbent For Sulfur.
Final Technical Report - September 1, 1992 through August 21, 1993.
Swisher, James H.
Illinois Clean Coal Institute
In this pdf format, this
document has 31 pages and is 1.77 MB.
Table
of Contents
|
1. |
Abstract |
1 |
|
2. |
Executive Summary |
2 |
|
3. |
Objectives |
4 |
|
4. |
Introduction and Background |
4 |
|
5. |
Experimental Procedures |
5 |
|
6. |
Results and Discussion |
7 |
|
6.1 |
Properties of 75%Zn2TiO4-25%TiO2 Sorbents made from fine powders |
9 |
|
6.2 |
Properties of 50%Zn2TiO4-50%TiO2 Sorbents made from fine powders |
11 |
|
6.3 |
Properties of 50%Zn2TiO4-50%TiO2 Sorbents made from coarse powders |
15 |
|
6.4 |
Surface Area Measurements |
20 |
|
6.5 |
Sulfidation-Regeneration Tests in Simulated Coal Gas |
20 |
|
6.6 |
Crush Strength Comparisons |
22 |
|
7. |
Conclusions and Recommendations |
24 |
|
8. |
Acknowledgements |
25 |
|
9. |
References |
26 |
|
10. |
Project Management Report |
28 |
|
11. |
Projected and Estimated Expenditures by Quarter |
29 |
|
12. |
Costs by Quarter |
30 |
|
13. |
Schedule of Project Milestones |
31 |
|